assembling and sale of machines and plates for pad print, industrial pad print, clichè, pad print, pad printing accessoriespad printing machines, pad print, pads, clichè, plates for pad print, pad print, pad print, pad printing machines, sale of pad printing accessories, pad printing consumables, sale, accessoriespad printing machines, pad print, pads, clichè, plates for pad print, pad print, pad print, pad printing machines, sale of pad printing accessories, pad printing consumables, sale, accessoriesComec Italia srl, Varese, Italy - Assembling and sale of machines and plates for pad printComec Italia srl, Varese, Italy - Assembling and sale of machines and plates for pad print




 

 








PLT7 Ink

 

 

FEATURES:
It is a two-component ink.
It has a glossy appearance and is quick drying.
Its main feature is the high mechanical and chemical resistance.
Non-toxic ink (NT) in compliance with the EN 71/part 3 European standard.

PRINTING SUPPORT:

It is particularly indicated for the printing on the following materials: thermosetting resins, polyamides, polycarbonates, polyesters, polymethyl methacrylates, polystyrene, ABS, polyurethanes and stiff PVC.
It can also be utilised, getting good results, on glass, metal, enamelled surfaces and polyethylenepolypropylene (pre-treated)

RESISTANCE:
Excellent resistance to a large number of organic solvents, chemical products and diluted acids.
It has a very good abrasion resistance.

FLASH POINT
Higher than 43°C

PREPARATION:
Mix the ink with the PLH catalyst in a 3:1 ratio (3 parts ink and 1 part catalyst)

CAUTION!
The catalyzed ink must be consumed within 6-8 hours or afterwards it gradually loses its mechanical-chemical resistance and its ability to adhere to the support.


Mix and strongly dilute the ink by using the PLA thinner in the measure of max. 10-20%.
When printing fine details or screened images (e.g. 80/ 120 lines per cm) in warm environments, we recommend you add the PLD retardant in a minimum percentage.

CAUTION!
Excessive dilution generates a loss of the covering power, smudges and an imperfect detachment of the ink from the pad.
An insufficient dilution causes problems of drawing the ink from the cliché, printing repeatability and dripping of the ink with a consequent decline of the printing quality.


DRYING AND HARDENING
The drying time lasts 2 minutes at an ambient temperature of about 20°C.
If you would like it to dry in only a few seconds, you can use hot air circulation ovens (60-80 b °C) or high temperature spot devices (air or infrared rays) that can be installed on the piece feeding systems (e.g. rotary tables, conveyors, etc.).
The ink is completely hardened after 4-5 days.

COLOUR RANGE:
Consult the COMEC colour chart of glossy hues that includes a selection of 24 standard colours plus 3 threecolour shades.
All of the colour shades can be mixed with each other.
Upon request:
  • special sample colours.
  • metallic gold and silver shades ready for use.
ADDITIVES:
PLA thinner.
PLD retardant.
PPLD retardant paste.
PLH catalyst.
PLT7/70 transparent base.
OP opacifier.

PRESERVATION:
Lifetime of about 2 years.
Conditions for preservation: the package must be sealed tight and put in a dry and cool environment.

ATTENTION
The PLH catalyst must be preserved with the package sealed tight and put in a dry and cool environment. IT IS NOT MOISTURE-PROOF In the event it should become thick, it can no longer be used.